PPA (polyphthalamide) is a semi-aromatic polyamide: part of its polymer chain consists of aromatic rings derived from terephthalic or isophthalic acid. Compared with PA6 and PA66, it retains stiffness and strength at higher temperatures and absorbs less moisture, which is why it is used, almost always glass-filled, in under-the-hood automotive parts, electrical connectors and metal replacement components. The trade-off is a higher material cost than aliphatic nylons and higher processing temperatures.
Background and definition
Polyphthalamides were developed to fill the gap between aliphatic polyamides such as PA6 and PA66 and more expensive high-performance polymers. Their adoption was driven largely by the automotive industry, which needed materials able to replace metal in parts exposed to heat, oils and coolants. Well-known trade names include Amodel, Grivory HT, Zytel HTN and Vestamid HTplus.
ASTM D5336 defines PPA as a polyamide in which at least 55 mol% of the diacid portion of the repeating unit is terephthalic acid, isophthalic acid or a combination of the two. The designations describe the composition: "T" stands for terephthalic acid and "I" for isophthalic acid. Common examples are PA6T/66, PA6T/6I, PA6T/DT, PA9T and PA10T. For an overview of the whole family, see our guide to PA – polyamide (nylon).
Structure and grades
Like all polyamides, PPA contains amide groups (–CO–NH–) that form hydrogen bonds between chains. The aromatic rings stiffen the chain: glass transition and melting temperatures rise compared with aliphatic polyamides, and the share of water-absorbing amide groups goes down.
Most PPA injection molding grades are semi-crystalline. When isophthalic acid makes up most of the diacid portion, the polymer becomes amorphous: amorphous grades shrink more uniformly but have lower chemical resistance.
PPA is rarely molded unfilled. The most common formulations are:
- Glass-filled: the most widely used version, often with high glass fiber loadings. It provides the stiffness and strength needed for structural parts and metal replacement.
- Mineral-filled or glass/mineral-filled: more uniform shrinkage and less warpage than glass fiber alone.
- Carbon fiber-reinforced: high stiffness at low weight.
- Flame-retardant: including halogen-free grades for electrical and electronic applications.
- Heat-stabilized: for long-term exposure to high temperatures, for example in cooling systems.
- High-reflectance white: for LED reflectors and housings.
- Low mold temperature grades: formulated to crystallize in water-heated molds.
PPA vs PA66
| Property | PPA | PA66 |
|---|---|---|
| Chain structure | semi-aromatic | aliphatic |
| Stiffness at high temperature | higher | lower |
| Moisture absorption | lower | higher |
| Dimensional stability in humid environments | higher | lower |
| Toughness | lower | higher |
| Melt and mold temperatures | higher | lower |
| Material cost | higher | lower |
PPA advantages
- Retains stiffness and mechanical strength over a wider temperature range than PA6 and PA66, thanks to its higher glass transition temperature.
- Absorbs less moisture than aliphatic polyamides: part dimensions, stiffness and electrical properties vary less with ambient conditions.
- Good creep and fatigue resistance, including at elevated temperatures.
- Resists oils, greases, fuels and glycol-based coolants, also at high temperature.
- Many grades withstand the lead-free reflow soldering cycles used for surface-mount (SMT) electronic components.
- Flame-retardant grades are available, including halogen-free ones.
- Glass-filled grades replace metals such as die-cast aluminum in many components: they cut weight, allow several functions to be integrated into one part and do not corrode.
PPA limitations
- It costs more than PA6 and PA66, so it pays off when aliphatic nylons fall short on temperature, humidity or dimensional stability.
- It is processed at melt temperatures above 300 °C (570 °F) and, for many grades, in oil-heated molds: it needs suitable equipment and tight process control.
- It is still a polyamide: less hygroscopic than PA66, but it must be dried before molding.
- Toughness and elongation at break are lower than those of aliphatic polyamides, especially in highly filled grades.
- In glass-filled grades, shrinkage differs in the flow and cross-flow directions: without careful part and mold design, the part warps.
- Glass fiber is abrasive: hardened tool steels are needed in high-wear areas of the mold.
- It does not resist strong acids and oxidizing agents; compatibility with specific fluids must be checked against supplier data.
- For even higher service temperatures or harsher chemical environments, polymers such as PPS are worth evaluating.
Processing and injection molding
PPA is processed mainly by injection molding. Compared with aliphatic polyamides, the processing window is narrower and temperatures are higher, so these points matter most:
- Drying: pellets must be dried in a desiccant dryer, typically at around 120 °C (250 °F) for a few hours, down to the residual moisture specified by the supplier. At PPA processing temperatures, residual moisture causes splay, bubbles and hydrolysis of the polymer, with a loss of mechanical properties.
- Melt temperature: generally above 300 °C (570 °F), with values that vary widely from grade to grade. Barrel residence time should be kept short to avoid thermal degradation.
- Mold temperature: many semi-crystalline grades need a hot mold, often above 120 °C (250 °F), to crystallize fully. With a mold that is too cold, surface quality suffers and the part can show post-mold shrinkage and warpage in service. Low mold temperature grades widen the options, but the correct values are always those in the processing guide for the chosen grade.
- Tooling: very hot molds need insulating plates, fits and tolerances that account for thermal expansion, properly sized vents and abrasion-resistant steels. Gate locations and wall thicknesses should be designed to control fiber orientation and warpage.
- Material changes: before and after PPA, the barrel must be purged with a material suited to high temperatures, so that neither the previous nor the next polymer degrades.
In our plant, all 13 molding lines have a desiccant dryer, with molecular sieve dryers of the wheel or twin-tower type, and four lines have mold temperature controllers up to 180 °C (356 °F). Learn more about our plastic injection molding service: together with your engineering team, we assess whether the part really needs PPA or whether a glass-filled aliphatic polyamide such as PA6 is sufficient.
PPA applications
- Automotive: cooling system components such as thermostat housings and water pump parts, fuel system components, sensor and actuator housings, connectors, under-the-hood brackets and structural supports.
- Electric vehicles: connectors, thermal management components and insulating parts exposed to high temperatures.
- Electrical and electronics: SMT connectors, switch components, coil bobbins, LED reflectors and housings.
- Industrial: pump and valve components, fittings for hot fluids, gears and mechanical parts exposed to heat and chemicals.
- Household appliances: parts exposed to heat, steam and detergents.
Frequently asked questions
What is PPA?
PPA (polyphthalamide) is a semi-aromatic polyamide: under ASTM D5336, at least 55 mol% of its diacid portion is terephthalic acid, isophthalic acid or a combination of the two. The aromatic rings in the chain raise heat resistance and reduce moisture absorption compared with PA6 and PA66.
What is the difference between PPA and PA66?
PPA retains stiffness and strength at higher temperatures than PA66 and absorbs less moisture, so part dimensions and properties change less with the environment. In return it costs more, is less tough and needs higher melt and mold temperatures. If a glass-filled PA66 meets the requirements, it is usually the more economical choice.
Does PPA need to be dried before injection molding?
Yes: PPA is less hygroscopic than PA66 but still has to be dried in a desiccant dryer, typically at around 120 °C (250 °F) for a few hours, down to the residual moisture specified by the resin supplier. Wet pellets cause splay, bubbles and polymer degradation at PPA processing temperatures.
What mold temperature does PPA require?
Many semi-crystalline PPA grades need a hot mold, often above 120 °C (250 °F), to crystallize fully. A mold that is too cold can lead to poor surface finish, post-mold shrinkage and warpage in service. Some grades are formulated for lower mold temperatures; the correct value is the one in the processing guide for the chosen grade.
PPA or PPS: which one to choose?
It depends on the service environment: PPS absorbs very little moisture, is inherently flame-retardant and handles aggressive chemicals and long-term heat better, while PPA generally offers higher mechanical strength and toughness. For PPS we evaluate the material together with your engineering team; the full comparison is in our PPS guide.
Does Bemar Plast mold PPA?
Yes: PPA is one of the engineering polymers we injection mold. All 13 of our molding lines have a desiccant dryer, and four have mold temperature controllers up to 180 °C (356 °F), suitable for grades that require a hot mold. The service is described on our plastic injection molding page.